Getting Gold: A Gold-Mining Handbook for Practical Men
TO DETERMINE HEIGHTS OF OBJECTS.
By Shadows.
1. Set up vertically a stick of known length, and measure the length of its shadow upon a horizontal or other plane; measure also the length of the shadow thrown by the object whose height is required. Then it will be:—As the length of the stick’s shadow is to the length of the stick itself, so is the length of the shadow of the object to the object’s height.
By Reflection.
Place a vessel of water upon the ground and recede from it until you see the top of the object reflected from the surface of the water. Then it will be:—As your horizontal distance from the point of reflection is to the height of your eye above the reflecting surface, so is the horizontal distance of the foot of the object from the vessel to its altitude above the said surface.
Instrumentally.
Read the vertical angle, and multiply its natural tangent by the distance between instrument and foot of object; the result is the height.
When much accuracy is not required vertical angles can be measured by means of a quadrant of simple construction, represented in Fig. 46. The arc AB is a quadrant, graduated in degrees from B to A; C, the point from which the plummet P is suspended, being the centre of the quadrant.
When the sights AC are directed towards any object, S, the degrees in the arc, BP, are the measure of the angle of elevation, SAD, of the object.
TO FIND THE DEPTH OF A SHAFT.
Rule:—Square the number of seconds a stone takes to reach the bottom and multiply by 16.
Thus, if a stone takes 5 seconds to fall to the bottom of a shaft—
5² = 25 and 25 ° 16 = 400 feet, the required depth of shaft.
DESCRIPTION OF PLAN FOR RE-USING WATER.
Where water is scarce it may be necessary to use it repeatedly. In a case of this kind in Egypt, the Arab miners have adopted an ingenious method, which is shown in Fig. 47, and may be adapted to almost any set of conditions. At a is a sump or water-pit; b is an inclined plane on which the mineral is washed and whence the water escapes into a tank c; d is a conduit for taking the water back to a; e is a conduit or lever pump for raising the water. A certain amount of filtration could easily be managed during the passage from c to a.
COOLING COMPOUND FOR HEATED BEARINGS.
Mercurial ointment mixed with black cylinder oil and applied every quarter of an hour, or as often as expedient. The following is also recommended as a good cooling compound for heavy bearings:—Tallow 2 lb., plumbago 6 oz., sugar of lead 4 oz. Melt the tallow with gentle heat and add the other ingredients, stirring until cold.
CLEANING GREASY PLUMMER BLOCKS.
When, through carelessness or unpreventable causes, plummer blocks and other detachable portions of machinery become clogged with sticky deposits of grease and impurities, a simple mode of cleansing the same is to take about 1000 parts by weight of boiling water, to which add about 10 or 15 parts of ordinary washing soda. Keep the water on the boil and place therein the portions of the machine that are to be cleaned; this treatment has the effect of quickly loosening all grease, oil, and dirt, after which the metal is thoroughly washed and dried. The action of the lye is to form with the grease a soap soluble in water. To prevent lubricating oil hardening upon the parts of the machinery when in use, add a third part of kerosene.
PREVENTING SCALING AND PRIMING IN BOILERS.
Graphite “black-lead” added to the water in a boiler prevents scaling and priming. My method is to paint the inside of the boiler with a good coat of graphite mixed with water to the consistency of thin gruel, and let it stand till dry. It will not be amiss to give a second coat before getting up steam. Even if slight scaling has already taken place, the graphite particles will penetrate and the scale come away gradually.
CLEARING SCALE-STOPPED PIPES.
Where the water contains a large amount of mineral in solution, the pipes, particularly the small ones, inch to two inch, quickly become useless because of the rapid deposition of scale. I have seen in West Australia tons of small pipes thrown on to the scrap heap after a few months use, because of this difficulty. The treatment now indicated, which is my own invention, will make such pipes as good as new at small expense. Have a brick trough a little longer than your pipe. In this put a fire of wood, charcoal, coke, or a mixture of such fuel. Lay the pipes, a few at a time, in this. Heat slowly to cherry red. Then with pinchers suddenly immerse in a second trough of cold water, supporting one end above the water level. Most of the scale or incrustation will be violently ejected. With a long pipe, if the heat has not been regular, some may still adhere. Then usually tapping with a hammer will detach it. If not, a second heating and immersion will do so, leaving the interior as clean as when made. It is hardly necessary to add that ’tis best to stand clear of the ends when the explosion takes place.
AN EXCELLENT ANTI-FRICTION COMPOUND.
For use on cams and stamper shanks, which will be harmless should it drop into the mortar or stamper boxes, is graphite (black-lead) and soft soap. When the guides are wooden, the soft soap need not be added; graphite “black-lead” made into a paste with water will act admirably.
TO CLEAN BRASS.
Oxalic acid 1 oz., rotten stone 6 oz., powdered gum arabic ½ oz., sweet oil 1 oz. Rub on with a piece of rag.
A SOLVENT FOR RUST.
It is often very difficult, and sometimes impossible, to remove rust from articles made of iron. Those which are very thickly coated are most easily cleaned by being immersed in a nearly saturated solution of chloride of tin. The length of time they remain in this bath is determined by the thickness of the coating of rust. Generally from twelve to twenty-four hours is long enough.
TO PROTECT IRON AND STEEL FROM RUST.
The following method is but little known, although it deserves preference over many others. Add 7 oz. of quicklime to 1¾ pints of cold water. Let the mixture stand until the supernatant fluid is entirely clear. Then pour this off, and mix with it enough olive oil to form a thick cream, or rather to the consistency of melted and recongealed butter. Grease the articles of iron or steel with this compound, and then wrap them up in paper, or if this cannot be done, apply the mixture somewhat more thickly.
TO KEEP MACHINERY FROM RUSTING.
Take 1 oz. of camphor, dissolve it in 1 lb. of melted lard; mix with it (after removing the scum) as much fine graphite as will give it an iron colour; clean the machinery, and smear it with this mixture. After twenty-four hours rub off and clean with soft, linen cloth. This mixture will keep machinery clean for months under ordinary circumstances.
FIRE-LUTE.
An excellent fire-lute is made of eight parts sharp sand, two parts good clay, and one part horse-dung; mix and temper like mortar.
ROPE-SPLICING.
A short splice is made by unlaying the ends of two pieces of rope to a sufficient length, then interlaying them as in Fig. 48 (upper cut), draw them close and push the strands of one under the strands of the other several times as shown in the lower cut.
This splice makes a thick lump on the rope and is only used for slings, block-straps, cables, &c.
APPENDIX
(SELECTED DATA FOR MINING MEN)
TO FIND LOST PART OF VEIN
Zimmermann’s rule for finding the lost part of a vein on the other side of a vein, is as follows:—
Lay down upon paper the line of strike of lode and the line of strike of the fault (cross-course), and by construction ascertain the horizontal projection of the line of their intersection; from the point where the cross-course was struck by the lode, draw a line at right angles to the strike of the former and directed to its opposite wall. Notice on which side of the line of intersection this perpendicular falls, and after cutting through the cross-course, seek the “heaved” part of the lode on that side.
Thus let AB (Fig. 49) represent, at any depth, the line of strike of a fault or cross-course dipping east, and CD the line of strike of a lode dipping south, and we will suppose that in driving from C to D in a westerly direction, the fault has been met with at D. Knowing the dip of the lode and that of the fault, it is easy to lay down on any given scale, AₖBₖ and CₖDₖ, the lines of strike of the fault and lode respectively at a certain depth, say 10 fathoms, below AB. The point Dₗ, where AₖBₖ and CₖDₖ meet, is one point of the line of intersection. Join D and Dₗ, and prolong on both sides. The line MN represents the horizontal projection of the line of intersection of the two planes. At D erect DE at right angles and directed towards the opposite wall of the fault. As DE falls south of MN, the miner, after cutting through the fault, would drive in a southerly direction and eventually strike the lode again at F. It will be at once understood that if the miner were following the lode from b to F, the perpendicular would lie to the north of the line of intersection, and following the rule, he would drive in that direction, after cutting through the fault. When several faults in succession dislocate a lode, very great complications may arise.
THE CALCULATION OF ORE RESERVES. [4]
Having finished the survey of a metalliferous mine, the surveyor is sometimes called upon to calculate the quantity of ore reserves in that mine. Various methods are employed for this purpose.
[4] Bennett H. Brough’s “Treatise on Mine Surveying,” sixth edition, p. 165.
Indeed, different surveyors will not agree within wide limits as to the amount of ore reserves in the same mine. Sometimes the amount of ore in sight will be considered to be a rectangular block, limited by the outcrop of the vein, the depth of the shaft, and the extreme points of the levels, diminished by the amount extracted. Other surveyors would avoid so excessive an amount, and take but one-third of that amount.
The following method is recommended by Mr. J. G. Murphy, an experienced American mining engineer, as the fairest and most trustworthy:—
Let it be required to calculate the ore reserves in a mine opened up on a vein with a mean cross section of 6 feet; a cubic foot of the vein matter in place weighing 150 lb. The ore stopes are generally very irregular. In this case, however, it may be supposed that the stope faces are 11 feet apart and 8 feet high. There is an inclined shaft, 10 feet by 6 feet, following the dip of the vein, and six levels, each 7 feet by 6 feet, 100 feet apart. The lengths of the levels are—
| I. | 200 feet west 150 feet east. |
| II. | 160 feet west 100 feet east. |
| III. | 120 feet west 400 feet east. |
| IV. | 100 feet west 140 feet east. |
| V. | 165 feet west 180 feet east. |
| VI. | 350 feet west 150 feet east. |