SIMPLE WAY OF MAKING CHARCOAL.

Dig a pit 5 feet square by 3 feet deep and fill with fuel. After lighting, see that the pit is kept full. The hot embers will gradually sink to the bottom. The fuel should be kept burning fiercely until the pit seems almost full, when more fuel should be added, raising the heap about a foot above the level of the ground. The earth dug out of the pit should then be shovelled back over the burning mass. After leaving it to cool for 24 hours the pit will be found nearly full of charcoal. About one-quarter the weight of the dry fuel used should be recovered in charcoal.

ROUGH SMELTING ON THE MINE.

Rough gold smelting on the mine is effected with a flux of borax, carbonate of soda, or, as I have often done, with some powdered white glass. When the gold is smelted and the flux has settled down quietly in a liquid state, the bulk of the latter may be removed, to facilitate pouring into the mould, by dipping an iron rod alternately into the flux and then into a little water, and knocking off the ball of congealed flux which adheres after each dip. This flux should, however, be crushed with a pestle and mortar and panned off, as, in certain cases, it may contain tiny globules of gold.

MISFIRES IN BLASTING.

One of the most common sources of accident in mining operations is due either to carelessness or to the use of defective material in blasting. A shot misses, generally for one of two reasons; either the explosive, the cap, or the fuse (most often the latter), is inferior or defective; or the charging is incompetently performed. Sometimes the fuse is not placed properly in the detonator, or the detonator is not properly enclosed in the cartridge, or the fuse is injured by improper tamping. If several shots have been fired together, particularly at the change of a “shift,” the men who have to remove the broken material may in so doing explode the missed charge. Or, more inexcusable still, men will often be so foolish as to try to clear out the drill hole and remove the missed cartridge. When a charge is known to have missed all that is necessary to do in order to discharge it safely is to remove a few inches of “tamping” from the top of the drill hole, place in the bore a plug of dynamite with cap and fuse attached, put an inch or two of tamping over it and fire, when the missed charge will also be exploded. Of course, judgment must be used and the depth of the drill taken into consideration. As a rule, miners use far more tamping than is at all requisite. The action of the charge will generally be found quite as effective with a few inches of covering matter as with a foot or more, while the exploding of misfire cartridges is rendered simple, as no removal of tamping is required before placing the top “plug” in case of misfire.

TO PREVENT LOSS OF RICH SPECIMENS IN BLASTING.

When blasting the cap of a lode, particularly on rich shutes of gold, the rock is apt to fly, and rich specimens may be thrown far afield and so be lost. A simple way of avoiding this is to procure a quantity of boughs, which tie into loose bundles, placing the leafy parts alternately end for end. Before firing, pile these bundles over the blast and, if care is used, very few stones will fly. The same device may be used in wide shallow shafts.

A SIMPLE MODE OF RETORTING SMALL QUANTITIES OF AMALGAM.

Clean your amalgam and squeeze it as hard as possible through strong calico or chamois leather. Take a large sound potato, cut off about a quarter from one end and scoop out a hole in the centre about twice as big as the ball of amalgam. Procure a piece of flat iron—an old spade will do as well as anything—insert the amalgam, and, having placed the potato, cut side downwards, thereon, put the plate of iron on the forge, heat up first gently, then stronger, till separation has taken place, when the gold will be found in a bright clean button on the plate and the mercury in fine globules in the potato, from which it can be re-collected by breaking up the partly or wholly cooked tuber under water in an enamelled or ordinary crockery basin. It is as well to place a piece of paper between the iron and the amalgam to prevent adhesion.

TO RETORT SMALL QUANTITIES OF MERCURY FOR AMALGAMATING ASSAY TESTS.

Fig. 34. Smoking-Pipe Retort.

Get two new tobacco pipes similar in shape (Fig. 34), with the biggest bowls and longest stems procurable. Break off the stem of one close to the bowl and fill the hole with well worked clay (some battery slimes make the best luting clay). Set the stemless pipe on end in a clay bed, and fill with amalgam, pass a bit of thin iron or copper wire beneath it, and bend the ends of the wire upwards. Now fit the whole pipe, bowl inverted, on to the under one, luting the edges of both well with clay. Twist the wire over the top with a pair of nippers till the two bowls are fitted closely together, and you have a retort that will stand any heat necessary to thoroughly distil mercury.

A SIMPLE MODE OF ASCERTAINING THE NOMINAL HORSE-POWER OF AN ENGINE.

Multiply the internal diameter of the cylinder by itself and strike off the last figure of the quotient. The diameter is

20” × 20”
20
-----
40ø.   The H.P. is 40.

The following rules will be found more professionally accurate from an engineering standpoint, though the term “horse-power” is not now generally employed.

To find the Nominal Horse-power.—For non-condensing engines: Multiply the square of the diameter of the cylinder in inches by 7 and divide the product by 80. For condensing engines: Multiply the square of the diameter of the cylinder in inches by 7 and divide the product by 200.

To find the Actual Horse-power of an engine, multiply the area of the cylinder in square inches by the average effective pressure in pounds per square inch, less 3 lb. per square inch as the frictional allowance, and also by the speed of the piston in feet per minute, dividing the product by 33,000, and the quotient will be the actual horse-power.

“SCALING” COPPER PLATES.

To “scale” copper plates they may be put over a charcoal or coke fire to slowly sublimate the quicksilver. Where possible, the fireplace of a spare boiler can be utilised, using a thin red fire. After the entire evaporation of the quicksilver the plates should be slowly cooled, rubbed with hydrochloric acid, and put in a damp place overnight, then rubbed with a solution of sal ammoniac and nitre in equal parts, and again heated slowly over a red fire. They must not be allowed to get red hot; the proper degree of heat is indicated by the gold scale rising in blisters, when the plates are to be taken from the fire and the gold scraped off. Any part of the plate on which the gold has not blistered should be again rubbed with the solution and fired. The gold scale should be collected in a glass or earthen dish and covered with nitric acid, till all the copper is dissolved, when the gold can be smelted in the usual way; but when it is molten, corrosive sublimate should be put in the crucible till a blue flame ceases to be given off.

A Second Method.

The simplest plan I know is to have a hole dug nine inches deep by about the size of the plate to be scaled; place a brick at each corner, and on each side, halfway between. Get up a good fire, and let it burn down to strong embers, or use charcoal, then place the plate on three bars of iron extending between the three pairs of bricks, have a strong solution of borax ready in which soak strips of old “table blanket,” laying these over the plate and sprinkling them with the borax solution when the plate gets too hot. After a time the deposit of mercury and gold on the plate will assume a white, efflorescent appearance, and may then be readily parted from the copper.

Another Method.

Heat the plate over an open fire, to drive off the mercury; after which, let it cool, and saturate with dilute sulphuric acid for three hours, or longer; then sprinkle over the surface a mixture of equal parts of common salt and sal ammoniac, and heat to redness. When cool, the gold scale comes off freely; the scale is then boiled in nitric or sulphuric acid, to remove the copper, previous to melting. Plates may be scaled about once in six months, and will under ordinary circumstances produce about one ounce of clean gold for each superficial foot of copper surface employed. I always paint the back of the plate with a mixture of boiled oil and turpentine, or beeswax dissolved in turpentine, to prevent the acid attacking the copper.

HOW TO SUPPLY MERCURY TO MORTAR BOXES.

I am indebted for the following to Mr. J. M. Drake, who, speaking of his experience on the Wentworth Mine, N.S.W., says: —

“Fully 90 per cent. of the gold is saved on the outside plates, only a small quantity remaining in the mortar. The plates have a slope of 2 in. to 1 ft. No wells are used, the amalgam traps saving any quicksilver which may leach off the plates. The quicksilver is added every hour in the mortar. The quantity is regulated by the mill manager in the following manner: Three pieces of wood, 8 in. wide by 12 in. long by 2 in. thick, have 32 holes 1 in. deep bored in each of them. These holes will just take a small 2 oz. phial. The mill manager puts the required quantity of quicksilver in each bottle and the batteryman empties one bottle in each mortar every hour; and puts it back in its hole upside down. Each block of wood lasts eight hours, the duration of one man’s shift.” This of course is for a 20-head mill with four mortars or “boxes.”

I commend this as an excellent mode of supplying the mercury to the boxes or mortars. The quantity to be added depends on circumstances. A careless battery attendant will often put in too much or too little when working without the automatic feeder. I have known an attendant on suddenly awaking to the fact half through his shift, that he had forgotten to put in any mercury, to then empty into the stamper box two or three pounds weight; with what effect may be easily surmised.

HOW WATER SHOULD ENTER STAMPER BOXES.

The following extract which relates to Californian Gold Mill practices is from Bulletin No. 6 of the California State Mining Bureau. I quite agree with the practice.

“The battery water should enter both sides of the mortar in an even quantity, and should be sufficient to keep a fairly thick pulp which will discharge freely through the grating or screen. About 120 cubic feet of water per ton of crushed ore may be considered an average, or 8 to 10 cubic feet per stamp per hour.

“Screens of different materials and with different orifices are used; the materials comprise wire cloth of brass or steel, tough Russian sheet iron, English tinned plate, and, quite recently, aluminium bronze. The ‘aluminium bronze’ plates are much longer lived than either of the other kinds, and have the further advantage that, when worn out, they can be sold for the value of the metal for remelting; these plates are bought and sold by the pound, and are said to contain 95 per cent. of copper and 5 per cent. of aluminium. Steel screens are not so much used, on account of their liability to rust.”