All public Sources
Public document

Account of the Skerryvore lighthouse

DocumentAdded to Pandi 21 November 2026
Reading progressPage 59 of 73

From this book

Fig. 100.

Mallet

Fig. 101.

Mould

During the process of raising with the peened side of the mallet, an external mould FGHF (fig. 101), with a needle-point P, at its vertex, is applied, to indicate its proper position with reference to the mould; and allowance is made on the height and diameter of the reflector to meet the expansion of the metal during the hard-hammering which is to follow. After each course of the raising with the wooden mallets, the reflector must be annealed in the following manner:—The reflector is first damped with clean water, and its surface dusted over with a powder, composed of one pint of powdered charcoal to one ounce of saltpetre, which is applied by means of a thin flannel bag. The reflector is then put on a clear charcoal fire, where it is turned round as the powder flies off, which is an indication that the metal is duly heated. Over-heating is very injurious. When removed from the fire, the reflector is plunged into a large tub, containing what is called the pickle, which is a solution of one quart of vitriol in five or six gallons of water. After this it is washed with clean water, and scoured with Calais sand.

The next step is to put the reflector, thus raised nearly to its true form, into an iron stool, where a small hole being drilled in its vertex, a circle is described from this point with a beam-compass, so as to cut the paraboloïd to the proposed size.

Fig. 102.

Planishing hammer

Fig. 103.

Planishing a mirror

Fig. 104.

Lighter hammer

Fig. 105.

Checking shape of lens

The reflector is next hard-hammered all over (or planished, as it is technically termed) on the bright steel-head a (fig. 103), with the planishing hammer (fig. 102); and to facilitate working, the reflector is slung in a flexible frame SS, and counterbalanced by a weight w, hanging by a cord over the pulleys p p. When the reflector is all planished over, the next process is the smoothing, which is done on the steel-head a, with a lighter hammer (fig. 104 ), muffled with fine parchment at each end. After it is smoothed comes the finishing, or what is called the filling up to the mould. This is a tedious process, and the workman requires continually to have recourse to the marble table at M, on which he lays the reflector, as shewn in fig. 105, and applies to successive portions of its surface the mould g n, which has a needle-point centred at n, in the small hole drilled in the vertex. During this examination, he marks with a fine slate-pencil those portions of the reflector which do not meet the mould g n. The parts, so marked, are gently gone over with the muffled hammer, until every point touches the mould. This last process requires great caution; for, if any part of the surface be raised above the gauge, it is hardly possible to remedy it. Such a mistake, indeed, can only be corrected by annealing the reflector afresh, and bringing it back to the true form with the mallet; but reflectors so cobbled are never good. The table M (fig. 105) rests on a square box C, in which the tools and moulds are kept.

Fig. 106.

Apparatus to adjust burner

When thus finished from the hammer, the reflector is put into the apparatus shewn in fig. 106, which is placed at the end of a long dark corridor. RR is a wooden frame fixed to the wall with projecting brackets at K, which carry the reflector, fixed at E, E, by means of screws, so as always to have a definite position with reference to the bracket B, which carries the lamp and its fountain f, so arranged that its flame may admit of perfect adjustment to the point which ought to be the focus of the reflector. For the purpose of this adjustment, S shews screws for raising and depressing the level of the burner; and the lines or marks M, M′ shewn at the sockets J being brought into line, regulate the position of the burner in the plane of the focus, after it has been raised to the level of that plane by means of the screws at S. The lamp being lighted and thus properly placed, its effect on the reflector’s surface is observed by some one stationed at a convenient distance; and if the whole surface appear luminous, the instrument is considered fit for polishing; but if any dark spaces be found in it, the whole reflector must be again carefully tested by means of the mould, and the defective parts remedied in the manner above described.

The next step is to turn over the edge of the reflector, so as to stiffen it. For this purpose it is placed in the matrix P′P′ (fig. 107), and the needle-point at V is adjusted by the screw at D, so as just to enter the small hole formerly drilled in the vertex of the reflector. The die-plate PP (which is worked by means of the arms AA, which turn the screw S) then descends and presses the edge over, which is finished with a finely polished tool C, revolving round the axis of the instrument, which coincides with the centre of the matrix and die. In order to ensure a steady vertical movement of the die-plate PP, cross-arms FF, which are provided with sockets HH, which slide over the rods GG, GG, are added to prevent any lateral shake or derangement. The whole frame is stiffened by the cross-head in which the screw S works.

Fig. 107.

Matrix for edge stiffening

Fig. 108.

Cast-iron polishing table

Fig. 109.

Cast-iron polishing table

The reflector is then placed on the circular cast-iron table (figs. 108, 109), to which it is attached by the clamp-screws S, S. In this position, the bizzle W (fig. 108) and back-belt NAN (fig. 109), are soldered on. After this the reflector is ready for being finally polished; for which purpose, it is placed in a chaise percée, padded round the edges, and is first scoured all over with a piece of pure charcoal of hard wood, and next with a mixture of Florence oil and finely washed rottenstone, applied by means of a large ball of superfine cloth. It is then carefully cleansed with a piece of fine flannel dipped in Florence oil, and afterwards dusted over with the powder of well washed whiting, and wiped out with a soft cotton cloth. Lastly, it is carefully rubbed by the naked hand, with finely washed rouge and clean water, and wiped with a smooth chamois skin. In all the polishing and cleansing processes, some skill in manipulation is required, as the hand is generally moved in such a manner as to describe successive circles with their planes parallel to the lips of the reflector, and their centres in the axis of the generating curve.

The prices paid to the workmen for the various departments of the reflector-making are generally as follows:—

Raising the plate to the curve, with the wooden mallet,L.0100
Hammering and smoothing to the mould,150
Finishing in the die, and putting on bizzle and back-belt,060
Polishing,0120
 L.2130

The prices paid to the manufacturer were for the large reflectors of 24 inches aperture, L.43; for the small ones of 21 inches, L.31, 12s. The lamp with the sliding-carriage, required for each, costs L.6.

APPENDIX, No. III. NOTES ON THE GRINDING OF THE VARIOUS PIECES COMPOSING THE INSTRUMENTS USED IN DIOPTRIC LIGHTHOUSES, CHIEFLY FROM NOTES FURNISHED BY M. THEODORE LETOURNEAU OF PARIS.

The glass used in all the parts of the optical apparatus of the dioptric Lighthouses is that of St Gobain, whose index of refraction is 1·51.

As well on account of the difficulty experienced in producing at all times regular castings of glass from the moulds, as in order to compensate for the frequent accidents, which occur in the first application of the rubbers to the inequalities of the surface of the glass, the castings, whether for rings of lenses or prisms, are made from moulds, exceeding the intended size of the finished pieces by one-eighth part.

We shall take as an example, which is well calculated to illustrate the difficulties of the grinding process, one of the prismatic rings of a Catadioptric Light of the first order. The first operation will be to take off the rough arris at the angles of the pieces as they come from the moulds, and to reduce to equality the length of each of the four quadrantal prisms or segments by removing from each the quantity that may be necessary to make those four pieces, when placed on a circle, exactly equal to that of the finished zones. Each of them must have an excess of material at the various surfaces just sufficient to insure the rubber having scope enough to remove all the flaws or defects of the two surfaces to be first ground, which are the (concave and convex) refracting faces of the zone (the sides AC and BC in the Table in the Appendix, No. IV.)

Fig. 110.

Lens pieces on lathe table

The pieces must be placed end to end on the horizontal plane or table of the lathe at AA (fig. 110), and must rest on the exterior arris A of the reflecting side, on which arris there is ground a narrow plane whose width is proportionate to the projection of the outer edge beyond the inner edge of the zone, foreshortened by the bevel or inclination of the reflecting side, when resting (as in fig. 110) on the circular iron belt, which is screwed to the table of the lathe provided for its reception. This narrow plane at the arris A should be sufficient to give the prism a solid and regular bearing on the circular iron belt. In this figure (fig. 110) a b is the vertical axis of the lathe, n the point from which the co-ordinates for O, the grinding centre for the exterior concave refracting surface AC, are measured, and e AC the arc swept by the grinding surface. Conversely, n′ is the origin of the co-ordinates for the grinding centre O of the interior convex refracting surface BC, and e CB the arc swept by its grinding surface. Some skill is required in fixing the prism on the belt, for, on the one hand, there is an obstacle to correct workmanship from the dragging motion of the platform, and, on the other, by the unequal subdivision of the weight of the glass, which should be nearly balanced. This narrow plane being perfectly adjusted for all the segments so as to bed them quite level, the circular iron belt on which the ring should be ground, is placed on its platform, in the manner represented in the figure. It should be as truly levelled as possible, otherwise all the subsequent operations will be deranged by it. This iron belt is heated by means of heating pans; and the degree of heat may be practically judged of by the ebullition of drops of water let fall on it. The segments of glass are also at the same time placed in a stove heated with steam, and are generally raised to about 120° centigrade. The difference between the time required for the two operations of heating the iron belt and the glass segments is employed in laying or bedding a quantity of cement on the reflecting side of the segment, so as to fill up the angular space between the glass and the iron belt, and also to serve as a seat for the segment in the manner shewn in fig. 110. This operation is performed on a plane surface, in order that the lower part of the mastic may be precisely on a level with the narrow plane already ground on the outer arris of the reflecting side. After being sure that the heat is equally spread over every part of the circular iron belt, the segment is arranged on it; and the workman must, at this juncture, exert all his skill in placing the parts of the segment in a position nearly concentric with the belt, or in a truly circular form, making due allowance, however, for the inequalities existing at various parts of the rough material, and at the same time taking care that there should be an interval of at least two millimètres (or about ¹⁄₁₂th inch) between the ends of each of the two adjacent segments. Without this interval the heat evolved during the polishing would either dilate the glass so much as to cause the ends of the segments to fly into splinters, or make it needful to remove the zone before this should take place, the inevitable consequence of which would be the fracture of the pieces. Those intervals between the segments are filled with statuary’s plaster, which must be carefully washed and brushed at each change of the emery employed in grinding.