We may assume, therefore, that the acids have the following effects on the stone:—

(1) They will not attack the parts coated with grease.

(2) They will penetrate more or less if the fatty coating is only thin.

(3) Where they touch the stone they dissolve it and eat it away.

(4) They give it a polish that facilitates printing. This polish disappears after a time on account of the cleaning with sponge or rag, but is replaced by a new polish produced by this very means.

(5) They do not prevent the adherence of fatty material later, as soon as the stone is dry, for which reason the parts prepared in the beginning with acid and gum arabic must be prepared again by renewed etching, to take the ink.

(6) Finally the acids have the property of giving to prepared stones that have been used for impressions, a rough surface instead of a polish when they are applied again, because they attack some parts more than others, producing little pores with sharp edges which catch the ink. This fact, as I will show more clearly later, makes necessary extraordinary care if one wishes to clean prepared plates or correct defects with new etching, because unskilled handling will often make them worse.

II THE ACIDS SPECIFICALLY

Nitric acid or aquafortis, muriatic acid, vinegar, tartaric acid, and acid of wood sorrel, all have nearly similar effects, but aquafortis and muriatic acid are used because of their greater cheapness.

Oil of vitriol or sulphuric acid, very much diluted with water, is available for light but not for extensive etching, because it transforms the surface of the stone into gypsum and deposits it again, so that after that the acid cannot penetrate at all, or only partially. If a part of vitriol, say diluted with twelve parts of water, is poured on a cleanly ground stone, there ensues a violent action which, however, is only brief. It might be supposed that the acid is sated with lime when it ceases to act, but if it is moved to another part of the stone it etches anew.

If the acid is washed from the stone and a woolen rag be used to rub it after it is dry, it takes on a mirror-like polish. In this dry condition it can be cleansed of color as easily as a copper plate, and if a stone thus polished is engraved with a steel tool, it is possible to make several impressions from it just as from copper. The polish is not lasting, however, because the skin of gypsum is very thin. But it is a useful method if it is desired to engrave the stone and ink it frequently to see the effect.

All the acids named have the property, previously mentioned, of etching the stone rough if it has been prepared before or used for impressions. It seems that the gum unites more strongly with some parts of the stone than with others, admitting the acid in these latter places. Possibly, also, the bubbles caused by etching may help to produce this roughness by hindering the uniform action of the acid. This seems to be confirmed by the fact that an etched stone, prepared with gum, does not get nearly so rough when etched again with very weak acid as it does when stronger fluid is used.

In still greater degree does this appear when using citric acid or a solution of alum in water. Take a finely ground stone, pour diluted aquafortis over it, prepare it with the gum solution, and then dry it thoroughly with a clean rag. Now pour a little citric acid or alum solution on parts of it and let it dry. Then paint the parts so treated with a fat or printing-ink. If the color is rubbed off with a wet rag, it will be seen that the stone has become white again in all places except those where the citric acid or alum are. Those parts will have taken the color exactly as if they had been painted with chemical ink. The same occurs when applying other acids, but in a lesser degree. This effect will be mentioned in future for many methods. Here I will remark only:—

It happens often that the stone takes color on places where it should remain clean. This is caused by clumsy handling, unclean rags, etc., and occurs particularly at the ends, because they dry first and are more exposed to careless manipulation. These smutted places usually can be cleansed with a clean woolen rag and gum solution or even with a wetted clean finger. But sometimes the defect will not yield so easily, especially if the printing-color is soft. Then the only remedy is to prepare the stone over again, and that is the time when one must have regard to the roughening that ensues, if the stone is not to be rendered worse instead of better.

Therefore it is best in such cases to polish the ends of the stone with pumice stone till all dirt is gone, and then to etch with diluted acid and prepare anew with gum arabic.

To be sure, it is possible to dip a clean woolen rag in strong, even pure acid, and thus etch dirt away from the ends; but great care is necessary that no drop may touch the design, as the ink that adheres to the latter is not strong enough to resist the acid. In thus cleansing the plate, the roughening is etched away by the violent action, and a new polish is obtained.

Still, in either method of cleaning dirty places, great care must be taken not to touch roughly, press, or rub with dirty fatty rags or with dirty, fatty fingers before the gum arabic is on it. The acid eats away all the previous material used in preparation, and leaves the plate practically in its clean, natural state. Consequently it will take on grease readily, and the application of gum is essential.

It is feasible to mix the gum directly with the acid solution, but this mixture must be made fresh again each day, as otherwise it loses much of its value.

The following points are important:—

First: If the grease remain long on a stone that, though prepared, has lost its coating of gum, it will penetrate the surface, and according to its amount and fluidity, will sink more or less into the stone, which will retain its polish on the surface but become more inclined to take dirt. It is better, therefore, to leave a small amount of gum coating on the stone in such cases.

Second: As only the extreme outer surface of the stone is prepared by the gum, and this is rubbed away gradually by wiping during the printing, so in the same proportion of wear and tear the original preparation would become lost, if it were not renewed from time to time, that is, if the stone were not again coated with gum. Twice a day, however, is enough.

Third: Because of this susceptibility of the surface to injury, a prepared stone must not be rubbed strongly with fatty material, because this damages the surface and the stone would readily soak up the fat.

Fourth: If a prepared plate is totally denuded of gum, and has been dry for a time, especially if it has already lost a part of the preparation through printing, it will incline very much to take color and smut. Therefore, when it is necessary to stop printing, it is well to coat the plate at once with gum, but only with a very thin coat. If this has not been done, and it is desired to use the plate again, great care must be taken to wet it with the very purest water, or, better still, with diluted etching fluid, for instance one part aquafortis to five hundred parts of water; and then to coat it with gum. To neglect this precaution may cause the total ruin of the plate. For safe-keeping of the plates, if they are to be used again for printing, the coating with gum is, therefore, absolutely necessary.

Fifth: Gum can prepare only a thoroughly clean stone or one properly etched. Therefore, if the surface of the stone has even the least trace of grease, it will take color, no matter how thickly it may be coated with gum. On this fact is based the method of transferring copper-plate impressions and other printed subjects, as will be described later.

Sixth: If the stone has had fat on its surface, and this fat has been etched away again, the power of the gum asserts itself, and the stone will be thoroughly prepared even if the fat has soaked considerably into the body of the stone.

Seventh: Mere grinding of the stone is not sufficient to attain a complete preparation through gum alone. Therefore, if an otherwise clean stone has some places after grinding where the fat has soaked in deeply, and one coats it with gum, the stone will take color after a time on these fatty places, as soon as the inked rag has been rubbed over the stone many times. However, this taking-on of color is only slight if the gum solution is thick, and long-continued cleaning will transform it into complete preparation.

Eighth: From both preceding observations we learn:—

Printing forces the color to sink considerably into the stone. If such a stone is required for new designs, it is not practicable to grind it so much that all the fatty places can be ground away. Therefore it is ground only till it is thoroughly even again. Then it must be well etched; otherwise it may happen that in printing the surface will rub away and the entire previous writing or design will appear again, a trouble hardly to be remedied.

If the stone is dirty in the middle, it can be cleaned in many cases by pouring on a few drops of oil of turpentine and the same quantity of gum solution, and rubbing it clean with a woolen rag. Then it must be washed with a wet sponge, after which it is inked. If it has not lost the smut, the only remedy is new preparation. As this must be done differently for each different lithographic style, it will be described in its place.

If fat has soaked well into the stone in places where it is not desired, it is always very difficult to remove it without injuring adjoining parts. Correction of crayon work, if it has been etched and used for printing, is especially difficult. It is true that the defective parts can be cut out easily with a sharp instrument, but then these places must be prepared again. If weak etching fluid is used, it will not suffice. If strong fluid is used, the fine parts are easily attacked, and at the same time the surface will become roughened so that the stone often blackens entirely in the corrected parts. To avoid this trouble, and to facilitate corrections, I made many experiments to discover an acid composition that should prepare a stone anew and perfectly and yet not roughen the surface. I found the best material in phosphoric acid, especially when mixed with finely crushed nutgall.

Water in which phosphorus has been kept a long time becomes acid and etches the stone. The acid can be obtained more quickly by burning the phosphorus and catching the smoke. This method is somewhat expensive, but one does not need much, as it is used only for correcting defects.

If a few drops of aquafortis or other acid are poured on a clean ground stone, it will be etched. Now wipe the etching fluid off clean and coat the plate with soap-water or chemical ink. As soon as it is dry, clean it of the fatty coating with a few drops of oil of turpentine. If it is dampened then with water and inked, it will take color everywhere, even at the etched places. If gum is mixed with the acid, the same result occurs, though the stone has been thoroughly prepared where this mixture touched it. From this it appears that soap-water (and the alkalis in general) can destroy the preparation given to the stone and make it receptive again to fats. It is different if phosphoric acid is used. This makes a preparation that can be destroyed only by very frequent coating of soapy water.

Continue reading