Navajo Silversmiths Second Annual Report of the Bureau of Ethnology to the Secretary of the Smithsonian Institution, 1880-1881, Government Printing Office, Washington, 1883, pages 167-178
Their iron pliers, hammers, and files they purchase from the whites. Pliers, both flat-pointed and round-pointed, are used as with us. Of files they usually employ only small sizes, and the varieties they prefer are the flat, triangular, and rat-tail. Files are used not only for their legitimate purposes, as with us, but the shanks serve for punches and the points for gravers, with which figures are engraved on silver.
The Indians usually make their own cold-chisels. These are not used where the scissors and file can be conveniently and economically employed. The re-entrant rectangles on the bracelet represented in Fig. 4, Pl. XIX, were cut with a cold-chisel and finished with a file.
Awls are used to mark figures on the silver. Often they cut out of paper a pattern, which they lay on the silver, tracing the outline with an awl. These tools are sometimes purchased and sometimes made by the Indians. I have seen one made from a broken knife which had been picked up around the fort. The blade had been ground down to a point.
Metallic hemispheres for beads and buttons are made in a concave matrix by means of a round-pointed bolt which I will call a die. These tools are always made by the Indians. On one bar of iron there may be many matrices of different sizes, only one die fitting the smallest concavity, is required to work the metal in all. In the picture of the smithy (Pl. XVII, in the right lower corner beside the tin-plate), a piece of an old horse-shoe may be seen in which a few matrices have been worked, and, beside it, the die used in connection with the matrices.
A little instrument employed in levelling the edges of the metallic hemispheres, is rude but effective. In one end of a cylinder of wood, about three or four inches long, is cut a small roundish cavity of such a size that it will hold the hemisphere tightly, but allow the uneven edges to project. The hemisphere is placed in this, and then rubbed on a flat piece of sandstone until the edges are worn level with the base of the wooden cylinder. The uses of the basin and the wooden stake are described further on.
Their method of preparing charcoal is much more expeditious than that usually employed by our charcoal-burners, but more wasteful; wood, however, need not yet be economized on the juniper-covered mesas of New Mexico. They build a large fire of dry juniper, and when it has ceased to flame and is reduced to a mass of glowing coals, they smother it well with earth and leave it to cool. If the fire is kindled at sunset, the charcoal is ready for use next morning.
The smith makes his own blow-pipe, out of brass, usually by beating a piece of thick brass wire into a flat strip, and then bending this into a tube. The pipe is about a foot long, slightly tapering and curved at one end; there is no arrangement for retaining the moisture proceeding from the mouth. These Indians do not understand our method of making an air chamber of the mouth; they blow with undistended cheeks, hence the current of air directed on the flame is intermitting. The flame used in soldering with the blow-pipe is derived from a thick braid of cotton rags soaked in mutton suet or other grease. Their borax is purchased from the whites, and from the same source is derived the fine wire with which they bind together the parts to be soldered. I have been told by reliable persons that it is not many years since the Navajos employed a flux mined by themselves in their own country; but, finding the pure borax introduced by the traders to be much better, they gradually abandoned the use of the former substance.
For polishing, they have sand-paper and emery-paper purchased from the whites; but as these are expensive, they are usually required only for the finishing touches, the first part of the work being done with powdered sandstone, sand, or ashes, all of which are used with or without water. At certain stages in the progress of the work, some articles are rubbed on a piece of sandstone to reduce the surfaces to smoothness; but the stone, in this instance, is more a substitute for the file than for the sand-paper. Perhaps I should say that the file is a substitute for the stone, for there is little doubt that stone, sand, and ashes preceded file and paper in the shop of the Indian smith.
For blanching the silver, when the forging is done, they use a mineral substance found in various parts of their country, which, I am informed by Mr. Taylor, of the Smithsonian Institution, is a "hydrous sulphate of alumina," called almogen. This they dissolve in water, in a metal basin, with the addition, sometimes, of salt. The silver, being first slightly heated in the forge, is boiled in this solution and in a short time becomes very white.
The processes of the Navajo silversmith may be best understood from descriptions of the ways in which he makes some of his silver ornament. I once engaged two of the best workmen in the tribe to come to Fort Wingate and work under my observation for a week. They put up their forge in a small outbuilding at night, and early next morning they were at work. Their labor was almost all performed while they were sitting or crouching on the ground in very constrained positions; yet I never saw men who worked harder or more steadily. They often labored from twelve to fifteen hours a day, eating their meals with dispatch and returning to their toil the moment they had done. Occasionally they stopped to roll a cigarette or consult about their work, but they lost very few moments in this way. They worked by the job and their prices were such that they earned about two dollars a day each.
The first thing they made was a powder charger with a handle in the shape of a dart (Fig. 2, Pl. XIX). Having cut in sandstone rock (Fig. 2, Pl. XVIII) the necessary grooves for molds and greased the same, they melted two Mexican dollars—one for the bowl or receptacle, and one for the handle—and poured each one into its appropriate mold. Then each smith went to work on a separate part; but they helped one another when necessary. The ingot cast for the receptacle was beaten into a plate (triangular in shape, with obtuse corners), of a size which the smith guessed would be large enough for his purpose. Before the process of bending was quite completed the margins that were to form the seam were straightened by clipping and filing so as to assume a pretty accurate contact, and when the bending was done, a small gap still left in the seam was filled with a shred of silver beaten in. The cone, at this stage, being indented and irregular, the workman thrust into it a conical stake or mandrel, which he had formed carefully out of hard wood, and with gentle taps of the hammer soon made the cone even and shapely. Next, withdrawing the stake, he laid on the seam a mixture of borax and minute clippings of silver moistened with saliva, put the article into the fire, seam up, blew with the bellows until the silver was at a dull red-heat, and then applied the blow-pipe and flame until the soldering was completed. In the meantime the other smith had, with hammer and file, wrought the handle until it was sufficiently formed to be joined to the receptacle, the base of the handle being filed down for a length of about a quarter of an inch so that it would fit tightly into the orifice at the apex of the receptacle. The two parts were then adjusted and bound firmly together with a fine wire passing in various directions, over the base of the cone, across the protuberances on the dart-shaped handle, and around both. This done, the parts were soldered together in the manner already described, the ring by which it is suspended was fastened on, the edge of the receptacle was clipped and filed, and the whole was brought into good shape with file, sand, emery-paper, &c.
The chasing was the next process. To make the round indentations on the handle, one smith held the article on the anvil while the other applied the point of the shank of a file—previously rounded—and struck the file with a hammer. The other figures were made with the sharpened point of a file, pushed forward with a zigzag motion of the hand. When the chasing was done the silver was blanched by the process before referred to, being occasionally taken from the boiling solution of almogen to be rubbed with ashes and sand. For about five hours both of the smiths worked together on this powder-charger; subsequently, for about three hours' more, there was only one man engaged on it; so that, in all, thirteen hours labor was spent in constructing it. Of this time, about ten hours were consumed in forging, about one and one-half hours in filing and rubbing, and about the same time in ornamenting and cleaning.
In making the hollow silver beads they did not melt the silver, but beat out a Mexican dollar until it was of the proper tenuity—frequently annealing it in the forge as the work advanced. When the plate was ready they carefully described on it, with an awl, a figure (which, by courtesy, we will call a circle) that they conjectured would include a disk large enough to make half a bead of the required size. The disk was then cut out with scissors, trimmed, and used as a pattern to cut other circular pieces by. One of the smiths proceeded to cut out the rest of the planchets, while his partner formed them into hollow hemispheres with his matrix and die. He did not put them at once into the cavity from which they were to get their final shape, but first worked them a little in one or more larger cavities, so as to bring them gradually to the desired form. Next the hemispheres were leveled at the edges by a method already described, and subsequently perforated by holding them, convex surface downwards, on a piece of wood, and driving through them the shank of a file with blows of a hammer. By this means of boring, a neck was left projecting from the hole, which was not filed off until the soldering was done. The hemispheres were now strung or, I may say, spitted on a stout wire in pairs forming globes. The wire or spit referred to was bent at one end and supplied with a washer to keep the heads from slipping off, and all the pieces being pressed closely together were secured in position by many wraps of finer wire at the other end of the spit. The mixture of borax, saliva, and silver was next applied to the seams of all the beads; they were put into the fire and all soldered at one operation. When taken from the fire they were finished by filing, polishing and blanching.